With PMC® Flex™, you can work, roll, cut and shape this fine silver metal clay like modeling clay and enjoy a much longer working time--weeks, if need be! The clay firms up somewhat but stays pliable enough to bend, twist, shape--even join edges with slip--up to a month later (NOTE: You won't be able to ball-up and re-roll the clay; to do that, you'll need to rehydrate the clay and begin again). Then, when you're ready, fire the clay to produce a pure fine-silver object. This variety of PMC silver clay is ideal for use in the classroom and for anyone new to working with metal clay; its extended window of working time gives you (or your students) ample time to get designs just the way you want them.
Composition: Metal powder (90%), water and organic binder (10%) Shrinkage: 15% Color: Pickle white Physical Properties: • Firing temp.: 1,650°F (900°C) for two hours to achieve highest hardness and maximum durability; or 1,110°F (600°C) for 45 minutes; or 1,200°F (650°C) for 20 minutes; or 1,290°F (700°C) for 10 minutes. • Melting point: 1,762°F (960°C) • Density after firing: 9.3 specific gravity (rolled silver = 10.5 specific gravity) Package contains 30 g. of metal.
- PMC FLEX Silver Clay
Size: 30 grams Composition: Metal powder (90%), water and organic binder (10%) Shrinkage: 15% Color: Pickle white Physical Properties: • Firing temp.: 1,650°F (900°C) for two hours to achieve highest hardness and maximum durability; or 1,110°F (600°C) for 45 minutes; or 1,200°F (650°C) for 20 minutes; or 1,290°F (700°C) for 10 minutes. • Melting point: 1,762°F (960°C) • Density after firing: 9.3 specific gravity (rolled silver = 10.5 specific gravity) Package contains 30 g. of metal.
|
|
|
|
|
|
|