A quick and effective method of cleaning objects prior to plating. The cleaning process uses an electrolytic bath, similar to plating operations. The 2 lb. size makes 8 gallons. Use with a stainless steel anode. Clean with the solution heated from 120° to 160° F (50° to 71° C) at 2 to 6 volts for 15 to 30 seconds.